Ce-TZP Cerium Stabilized Zirconia Beads
Zirconia toughened ceramics prepared with cerium oxide as stabilizer. Generally, the doping mole fraction of cerium oxide is between 8% and 16%. The preparation process, toughening mechanism and yttrium oxide stabilized zirconia ceramics are basically the same, which has strong resistance to hydrothermal aging, and its application range is similar.
-
ISAMill Mining ceramic grinding media ball
SANXIN provides ceramic grinding media from 2008, offers density 4.5g/cm³ compound balls, and alumina balls for mineral mining, high efficiency with low wear loss.
넶19 2022-10-25 -
Ceramic grinding balls in grinding GCC, achieve fine particle size(8-25μ in Wolkem)
SANXIN New Material provides zirconia compound ZTA balls and alumina balls for GCC grinding.
넶22 2022-10-25 -
The grinding effect of zirconia beads with different particle sizes on the suspension agent
Using sanding media of different particle sizes, the sanding effects obtained are different.
넶19 2022-10-25